Type of CoatingType of CoatingThi ckness (jum)Neutral SaltSpray Test (h)Temperature & HumidityTest (h)PCT/HAST(h)Operating Temperature (°C)
Zn(Bluish white)4~15≤24//≤160
Zn(Colored)4~15≤48//≤160
Ni(Barrel Plating)5~20≤48≤168≤48≤200
Ni(Rack Plating)5~20≤16≤168≤48≤200
NiCuNi(Barrel Plating)5~20≤48≤168≤48≤200
NiCuNi(Rack Plating)5~20≤16≤168≤48≤200
Epoxy5~20≤72≤72≤48≤160
Ni+Epoxy10~30≤500≤500≤200≤160
NiCu+EpOXy10~30≤500≤500≤200≤160
Ni+Sn5~20≤72≤168≤96≤200
Ni+Ag5~20≤72≤168≤96≤160
Ni+AU5~20≤72≤168≤96≤200
NiCuNi+Sn5~20≤72≤168≤96≤200
Ni+AP.Ni(Barrel Plating)3~20≤72≤168≤48≤160
Ni+AP.Ni(Rack Plating)3~20≤24≤168≤48≤160
PVD.AI2~15≤24≤168≤24≤400
The specific corrosion resistance of different products depends on the productspecifications. in general,temperature & humidity test and PCT/HAST tests are not conducted

Smco Magnet Plating Requirement

Type of CoatingType of Coating Thickness (μm)Neutral SaltSpray Test (h)Temperature & Humidity Test (h)PCT/HAST(h)Operating Temperature (°C)
Zn(Bluish white)4~15≤24//≤160
Zn(Colored)4~15≤48//≤160
Ni(Barrel Plating)5~20≤48≤168≤48≤200
Ni(Rack Plating)5~20≤16≤168≤48≤200
NiCuNi(Barrel Plating)5~20≤48≤168≤48≤200
NiCuNi(Rack Plating)5~20≤16≤168≤48≤200
Epoxy5~20≤72≤72≤48≤160
Ni+Epoxy10~30≤500≤500≤200≤160
NiCu+EpOXy10~30≤500≤500≤200≤160
Ni+Sn5~20≤72≤168≤96≤200
Ni+Ag5~20≤72≤168≤96≤160
Ni+AU5~20≤72≤168≤96≤200
NiCuNi+Sn5~20≤72≤168≤96≤200
Ni+AP.Ni(Barrel Plating)3~20≤72≤168≤48≤160
Ni+AP.Ni(Rack Plating)3~20≤24≤168≤48≤160
PVD.AI2~15≤24≤168≤24≤400